Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.692 GPa @Temperature -50.0 °C |
390.4 ksi @Temperature -58.0 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B140 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B140 NC010 is a 40% mineral reinforced polyamide 66 for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |