Polymer Property : Shear Modulus = 392 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 2.70 GPa

@Temperature 232 °C
392 ksi

@Temperature 450 °F
T300; In Plane; AMB
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel
Shear Modulus 2.70 GPa

@Temperature 232 °C
392 ksi

@Temperature 450 °F
AS4C; In Plane
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel