Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 4.50 GPa @Temperature 23.0 °C |
653 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |
|||
Shear Modulus | 4.50 GPa @Temperature 23.0 °C |
653 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |