Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.280 GPa @Temperature 90.0 °C |
40.6 ksi @Temperature 194 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |