Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.307 GPa @Temperature 20.0 °C |
44.5 ksi @Temperature 68.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |