Shear Modulus 3.307 GPa

@Temperature -20.0 °C
479.6 ksi

@Temperature -4.00 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935 BK505 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced Polyethylene Terephthalate Rynite 935 BK505 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti..