Polymer Property : Shear Modulus = 5.09 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.0351 GPa

@Temperature 160 °C
5.09 ksi

@Temperature 320 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100ST BK602 Acetal (POM)  (Unverified Data**)