Mechanical Properties Metric English Comments
Shear Modulus 60.3 GPa

@Temperature 200 °C
8750 ksi

@Temperature 392 °F
Special Metals INCOLOY® Alloy 903
A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a..
Shear Modulus 60.3 GPa

@Temperature 450 °C
8750 ksi

@Temperature 842 °F
Special Metals INCOLOY® Alloy 903
A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a..