Shear Modulus 61.4 GPa

@Temperature 400 °C
8910 ksi

@Temperature 752 °F
Special Metals INCOLOY® Alloy 903
A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a..