Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 62.8 GPa @Temperature 538 °C |
9110 ksi @Temperature 1000 °F |
|
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt.. |