Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 65.0 GPa @Temperature 700 °C |
9430 ksi @Temperature 1290 °F |
Dynamic |
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 65.0 GPa @Temperature 700 °C |
9430 ksi @Temperature 1290 °F |
Dynamic |
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 65.0 GPa @Temperature 700 °C |
9430 ksi @Temperature 1290 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 65.0 GPa @Temperature 700 °C |
9430 ksi @Temperature 1290 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 65.0 GPa @Temperature 700 °C |
9430 ksi @Temperature 1290 °F |
Dynamic |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 65.0 GPa @Temperature 700 °C |
9430 ksi @Temperature 1290 °F |
Dynamic |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Shear Modulus | 65.0 GPa @Temperature 316 °C |
9430 ksi @Temperature 601 °F |
|
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt.. |
|||
Shear Modulus | 65.0 GPa @Temperature 700 °C |
9430 ksi @Temperature 1290 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
Shear Modulus | 65.0 GPa @Temperature 700 °C |
9430 ksi @Temperature 1290 °F |
Dynamic |
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |