Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 151 °C | 304 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East) LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re.. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 920 PC Opaque colors, low viscosity, superior flame retardance. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 920 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 920A PC Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 923 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 943A PC Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 943ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 920ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 940A PC Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 943 PC (Asia Pacific) Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 953 PC Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 953 PC (Asia Pacific) Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Vicat Softening Point | 151 °C @Load 5.10 kg |
304 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1201-05 Polycarbonate Resin Description: LUPOY PC 1201-05 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 151 °C | 304 °F | B/120; ISO R306 |
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 151 °C @Load 5.10 kg |
304 °F @Load 11.2 lb |
Rate A (50°C/h); ASTM D1525 |
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Vicat Softening Point | 151 °C | 304 °F | |
Styron CALIBRE™ 891 10 Polycarbonate, General Purpose CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc.. |
|||
Vicat Softening Point | 151 °C | 304 °F | 50°C/hr, 50N; ASTM D1525 |
Styron EMERGEâ„¢ 4800-10 Polycarbonate EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
Vicat Softening Point | 151 °C | 304 °F | 50°C/hr, 50N; ASTM D1525 |
Styron EMERGEâ„¢ 4330-6 Polycarbonate EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information .. |
|||
Vicat Softening Point | 151 °C | 304 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® K-1300Y Standard (mold release/ice color grade) Polycarbonate Resin Extrusion molding, blow molding and thick-wall injection molding grade. It has a improved mold release property and is bluish-tinted to exhibit clear color.Applications:Extruded products such as she.. |
|||
Vicat Softening Point | 151 °C | 304 °F | A50 (10N); ISO 306 |
Domo 2300L Polypropylene Copolymer Information provided by Domo. |
|||
Vicat Softening Point | 151 °C @Load 1.02 kg |
304 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem PD 943XP HOMO Polypropylene Homopolymer PD 943XP is a medium melt flow rate homopolymer with slip and antiblocking agents. It is suitable for blown film extrusion. This product features good impact strength, excellent gloss and transparen.. |
|||
Vicat Softening Point | 151 °C | 304 °F | ISO 306/A50 |
Addiplast Addilene PMD 50258 Polypropylene Copolymer For electroplatingInformation provided by Addiplast. |
|||
Vicat Softening Point | 151 °C | 304 °F | ISO 306/A50 |
Addiplast Addilene J 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Vicat Softening Point | 151 °C @Load 5.10 kg |
304 °F @Load 11.2 lb |
ISO 306 |
Radici Heraform® R 3000 Acetal Copolymer Very easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Radici group. |
|||
Vicat Softening Point | 151 °C @Load 5.10 kg |
304 °F @Load 11.2 lb |
ISO 306 |
Radici Heraform® R 350 Acetal Copolymer Standard grade for injection molding of thick wall parts, stiff-flowing, extrusion grade for tubes and sheet.Information provided by Radici group. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 940 PC Opaque colors, medium viscosity, superior flame retardance. |