Material Notes:
Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance, heat distortion resistance and optical clarity as well as high melt strength for sheet extrusion application. The CALIBREâ„¢ 200-6 series products are available in 4 additive packages: CALIBREâ„¢ 200: No mold release or UV Stabilizer. CALIBREâ„¢ 201: Mold release. CALIBREâ„¢ 202: UV stabilizer. CALIBREâ„¢ 203: Mold release and UV stabilizer. (Note that CALIBRE 202 and 203 grades are not available in Europe and do not comply with EU food contact regulations)Applications:Small and large applianceBeverage containers/service wareLiquid containersFood processor housingsCustom sheetPackaging applicationsGovt. and Industry Standards:US FDA 21 CFR 177.1580CSAUnderwriters Laboratory (UL)EU food contact 2002/72/ECInformation provided by Styron
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/A; ASTM D792
Water Absorption 0.32 %

@Temperature 23.0 °C
0.32 %

@Temperature 73.4 °F
Equilibrium, 50% RH; ISO 62; ASTM D570
0.15 %

@Temperature 23.0 °C,
Time 86400 sec
0.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ISO 294-4; ASTM D955
Melt Flow 6.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
6.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 73
73
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength at Break 72.0 MPa
10400 psi
ISO 527-2/50
72.4 MPa
10500 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638; ISO 527-2/50
Elongation at Break 150 %
150 %
50 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ASTM D638; ISO 527-2/50
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-2/50
2.41 GPa
350 ksi
50 mm/min; ASTM D638
Flexural Strength 96.5 MPa
14000 psi
Method I (3 point load), 2.0 mm/min; ASTM D790
97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Flexural Modulus 2.40 GPa
348 ksi
2.0 mm/min; ISO 178
2.41 GPa
350 ksi
Method I (3 point load), 2.0 mm/min; ASTM D790
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256; ISO 180/4A
Izod Impact, Notched (ISO) 93.0 kJ/m²

@Temperature 23.0 °C
44.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180
Tensile Impact Strength 588 kJ/m²
280 ft-lb/in²
ASTM D1822
Dart Drop, Total Energy 90.4 J
66.7 ft-lb
3.39 m/sec; ASTM D3763
Abrasion 45
45
[%] Taber; ASTM D1004
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Hot Ball Pressure Test 125 °C
257 °F
IEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Annealed; ASTM D648
146 °C
295 °F
Annealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
259 °F
Unannealed; ISO 75-2/A
129 °C
264 °F
Unannealed; ASTM D648
142 °C
288 °F
Annealed; ASTM D648
143 °C
289 °F
Annealed; ISO 75-2/A
Vicat Softening Point 151 °C

@Load 5.10 kg
304 °F

@Load 11.2 lb
Rate A (50°C/h); ASTM D1525
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0626 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Optical Properties Metric English Comments
Refractive Index 1.586
1.586
ASTM D542; ISO 489
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 60.0 Hz
3.0

@Frequency 60.0 Hz
ASTM D150
3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 50.0 Hz
0.0010

@Frequency 50.0 Hz
ASTM D150
0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 250 V

@Thickness 2.00 mm
250 V

@Thickness 0.0787 in
Solution A; IEC 60112
Descriptive Properties Value Comments
Average Extent of Burring 3 cm
ASTM D635
Copyright © lookpolymers.com All Rights Reserved