Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 43.3 °C | 110 °F | ASTM D1525 |
ExxonMobil OPTEMA™ TC 115 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 115 is an ethylene methyl acrylate copolymer, which can be used as a compatibilizer and impact modifier for engineering thermoplastics. It has been processed at temperatures up to 625°F w.. |
|||
Vicat Softening Point | 43.3 °C | 110 °F | ASTM D1525 |
ExxonMobil Escorene™ UL 7521 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7521 is a high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesiv.. |