Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 44.4 °C | 112 °F | ASTM D1525 |
ExxonMobil OPTEMA™ TC 130 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 130 is an ethylene methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compounds and.. |
|||
Vicat Softening Point | 44.4 °C | 112 °F | ASTM D1525 |
ExxonMobil Escorene™ UL 00328 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00328 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applications: Compoun.. |
|||
Vicat Softening Point | 44.4 °C | 112 °F | ASTM D1525 |
ExxonMobil Escorene™ FL 00328 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00328 is a copolymer of ethylene and vinyl acetate offering low gel. Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation. Machine.. |