Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 63.3 °C | 146 °F | ASTM D1525 |
ExxonMobil Escorene® LD 720.92 Specialty Film Resin
(discontinued **) Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |