Thermal Properties Metric English Comments
Vicat Softening Point 70.0 - 72.0 °C

@Load 5.00 kg
158 - 162 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RI 548/H Rigid PVC, Antishock Injection Molding
Electric antishock fittings