Polymer Property : Vicat Softening Point = 174 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 174 °C
345 °F
49 N; ISO 306, ASTM D1525
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
Vicat Softening Point 174 °C
345 °F
ASTM D1525
Samyang Triel® 5501BM Thermoplastics Polyetherester Elastomer, Blow Molding
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5501BM is for blow molding applications.Applications: Automotive BellowsInformation provided by Samyang...
Vicat Softening Point 174 °C
345 °F
Rate A/50; ISO 306
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Europe-Africa-Middle East)
NORYL PKN4752 is a translucent, high heat PPO+PS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food cont..
Vicat Softening Point 174 °C
345 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific)
Low odor grade for IC tray application
Vicat Softening Point 174 °C
345 °F
ASTM D1525
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene
This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c..
Vicat Softening Point 174 °C
345 °F
ASTM D1525
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene
This grade is highly recommended for film extrusion; also for injection molding, fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensiv..
Vicat Softening Point 174 °C
345 °F
ASTM D1525
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene
This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c..
Vicat Softening Point 174 °C
345 °F
ASTM D1525
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang.