Polymer Property : Vicat Softening Point = 180 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 410 Rigid PVC, Extrusion
Clic channels
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 625 Rigid PVC, Extrusion
Spiral pipes
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RH 207/OP Rigid PVC, Antishock Extrusion
Medium antishock satined profiles
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RH 208 Rigid PVC, Antishock Extrusion
Medium antishock profiles
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RH 210/K1 Rigid PVC, Antishock Extrusion
Antishock profiles
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RH 214 Rigid PVC, Antishock Extrusion
Antishock rolling shutters
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RH 612 Rigid PVC, Antishock Extrusion
Medium antishock profiles
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RH 704 Rigid PVC, Antishock Extrusion
Antishock spiral pipes
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RI 52 Rigid PVC, Injection Molding
Fittings for building trade
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RK 0758 Rigid PVC, Extrusion Lead Free
Electric corrugated pipes
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RK 912 Rigid PVC, Extrusion Lead Free
Spiral pipes
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RL 710 Rigid PVC, Extrusion
Corrugated electric pipes
Vicat Softening Point 67.0 - 82.0 °C
153 - 180 °F
Average value: 74.0 °C Grade Count:3
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 235 Rigid PVC, Extrusion
Electric channels and profiles
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 236 Rigid PVC, Extrusion
Electric channels