Thermal Properties Metric English Comments
Vicat Softening Point 182 °C
360 °F
50°C/h 50N
Covestro Apec® DP 1-9359/7 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer M..
Vicat Softening Point 182 °C
360 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem UR9076LG PEI
Standard flow mineral filled Polyetherimide Blend. Restricted sales to GE Specialty Film & Sheet.This data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 182 °C
360 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Vicat Softening Point 182 °C
360 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Vicat Softening Point 182 °C
360 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Vicat Softening Point 182 °C
360 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem ATX102R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 182 °C
360 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 182 °C
360 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region..
Vicat Softening Point 182 °C
360 °F
temperature A; ISO 306
Lubrizol ESTALOC® T514 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Vicat Softening Point 182 °C
360 °F
Covestro Apec® HT KU 1-9353 High-Heat Polycarbonate, UV-Stabilized
Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience..
Vicat Softening Point 182 °C
360 °F
Plastcom SLOVALEN PH 49 GF 60 PP reinforced with 60% glass fibre
Features: Modified homopolymer PP for injection moulding, chemically reinforced with 60% glass fibre, contains the modifier of mechanical properties.Very good strength and tensile modulus. Delivered..
Vicat Softening Point 182 °C
360 °F
ASTM D1525
PlastxWorld Veroplas PA2000 Nylon 6
general purpose, unfilled injection molding gradeInformation provided by PlastxWorld Inc.
Vicat Softening Point 182 °C
360 °F
ASTM D1525
PlastxWorld Veroplas PA2001F Nylon 6
flame retarded (UL94 VO), unfilled injection molding gradeInformation provided by PlastxWorld Inc.