Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 201 °C | 394 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 201 °C | 394 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 201 °C | 394 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 201 °C | 394 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 201 °C | 394 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 201 °C | 394 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |