Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 100.5 °C | 212.9 °F | ASTM D1525 |
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene SV - 0157 ABS extrusion grade has been formulated to provide excellent mechanical properties, extrusion stability, vacuum formability and chemical resistance. It has low flow with high impact streng.. |
|||
Vicat Softening Point | 100.5 °C | 212.9 °F | 50°C/hr, 50N; ISO 306-B50 |
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun .. |
|||
Vicat Softening Point | 100.5 °C | 212.9 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ABS VP-11 ELG Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc. |