Polymer Property : Vicat Softening Point = 235.6 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 235.6 °C
456.1 °F
ISO 306
Tisan TISAPET® 20% Glass Reinforced Polyethylene Terephthalate
Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a..