Polymer Property : Vicat Softening Point = 246 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 246 °C
475 °F
50°C/h 50N; ISO 306
LATI LARTON G/40 40% Glass Fiber Filled Polyphenylene sulfide (PPS)  (Unverified Data**)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..