Polymer Property : Vicat Softening Point = 26.7 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 26.7 °C
80.0 °F
ASTM D1525
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane
ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome..