Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 270 - 295 °C | 518 - 563 °F | Average value: 287 °C Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |