Thermal Properties Metric English Comments
Vicat Softening Point 37.2 °C
99.0 °F
ASTM D1525
ExxonMobil OPTEMA™ TC 140 Molding, extrusion, compounding and adhesive resin  (discontinued **)
OPTEMA TC 140 is a high flow, 21.5% methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compou..
Vicat Softening Point 37.2 - 78.0 °C
99.0 - 172 °F
Average value: 53.1 °C Grade Count:17
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an..