Thermal Properties Metric English Comments
Vicat Softening Point 38.0 °C

@Load 1.00 kg
100 °F

@Load 2.20 lb
ISO 306/A
Polimeri Europa Clearflex® CH G0 Very Low Density Polyethylene
Clearflex CH G0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has an excellent compatibility with polyolefins and fillers.Main Applic..
Vicat Softening Point 38.0 °C
100 °F
ASTM D1525
Huntsman IROGRAN® PS 456-202 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Vicat Softening Point 38.0 °C
100 °F
ASTM D1525
Dow Engage® 8180 Polyolefin Elastomer
Description: Engage® 8180 polyolefin elastomer is a lower density, high performance ethylene-octene copolymer that has excellent flow characteristics and provides good impact properties in blends w..
Vicat Softening Point 38.0 °C
100 °F
BASF Novolen® 2900 H Polypropylene
Injection molded and thermoformed parts.Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 38.0 - 95.0 °C
100 - 203 °F
Average value: 78.6 °C Grade Count:18
Overview of materials for Very Low Density Polyethylene (VLDPE)
This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va..
Vicat Softening Point 38.0 - 163 °C
100 - 325 °F
Average value: 94.5 °C Grade Count:63
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..