Thermal Properties Metric English Comments
Vicat Softening Point 130 - 195 °C
266 - 383 °F
Average value: 178 °C Grade Count:8
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Vicat Softening Point 135 - 195 °C
275 - 383 °F
Average value: 149 °C Grade Count:9
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..