Polymer Property : Vicat Softening Point = 387 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 197 °C
387 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
Vicat Softening Point 197 °C
387 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
Vicat Softening Point 197 °C
387 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA
Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to ..
Vicat Softening Point 197 °C
387 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA
Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to ..
Vicat Softening Point 197 °C
387 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
Vicat Softening Point 197 °C
387 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
Vicat Softening Point 197 °C
387 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East)
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
Vicat Softening Point 197 °C
387 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East)
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
Vicat Softening Point 197 °C
387 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Vicat Softening Point 197 °C
387 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Vicat Softening Point 197 °C
387 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..