Polymer Property : Vicat Softening Point = 504 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 262 °C
504 °F
Rate B/50; ISO 306
SABIC Innovative Plastics EXTEM UH1006 TPI Blend
High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha..
Vicat Softening Point 262 °C
504 °F
Rate B/120; ISO 306
SABIC Innovative Plastics EXTEM UH1006 TPI Blend
High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha..
Vicat Softening Point 262 °C
504 °F
Rate B/50; ISO 306
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 262 °C
504 °F
Rate B/120; ISO 306
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 262 °C
504 °F
Rate B/50; ISO 306
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 262 °C
504 °F
Rate B/120; ISO 306
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 262 °C
504 °F
Rate B/50; ISO 306
SABIC Innovative Plastics EXTEM UH1006M TPI Blend
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 262 °C
504 °F
Rate B/50; ISO 306
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 262 °C
504 °F
Rate B/50; ISO 306
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 262 °C
504 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Extem UH1016M TPI Blend
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 262 °C
504 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 262 °C
504 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Extem UH1016M TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.