Polymer Property : Vicat Softening Point = 626 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point >= 330 °C
>= 626 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1104/XCF/30 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
Vicat Softening Point >= 330 °C
>= 626 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1104-7824 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
Vicat Softening Point 330 °C
626 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..