Thermal Properties Metric English Comments
Vicat Softening Point 66.0 °C
151 °F
1000g; ASTM D-1525
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e..
Vicat Softening Point 66.0 °C
151 °F
ASTM D1525
DuPont Appeel® LSR11N704 Lidding Sealant Resin  (discontinued **)
Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal..
Vicat Softening Point 66.0 °C
151 °F
ASTM D1525
DuPont Appeel® LSR11D704 Lidding Sealant Resin  (discontinued **)
Appeel® LSR11D704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable s..
Vicat Softening Point 66.0 °C
151 °F
1000g; ASTM D-1525
ExxonMobil Escorene® LD-725 High EVA Film and Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An 18% vinyl acetate copolymer designed for specialty film and compounding applications. Outstanding sealability and low modulus are key attributes..
Vicat Softening Point 66.0 °C
151 °F
LyondellBasell Lupolen® 3652 D SW 00413 MDPE
Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Vicat Softening Point 66.0 °C
151 °F
ASTM D1525
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural Film, Shoe solesCSA No. 24937-78-8Information provided by LG Chemical
Vicat Softening Point 66.0 °C
151 °F
ISO 306B
Lucite International Elvakon® 4490 High Gloss Acrylic Capstock
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr..
Vicat Softening Point 66.0 °C
151 °F
A50; DIN 53460
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 66.0 °C
151 °F
Rate B, ASTM D1525-70
DuPont™ Surlyn® 9950 Ionomer Resin, Zinc
Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Vicat Softening Point 66.0 °C
151 °F
B50 (50N); ISO 306
Domo 2300L Polypropylene Copolymer
Information provided by Domo.
Vicat Softening Point 66.0 - 68.0 °C

@Load 5.00 kg
151 - 154 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds ART 0665/S Rigid PVC, Atoxic for General Purpose
Injection moulding and blow moulding bottles
Vicat Softening Point 66.0 °C
151 °F
ASTM D1525
C.O.I.M. LARIPUR® LPR7060 PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Vicat Softening Point 66.0 °C
151 °F
BASF Novolen® 2300 L Polypropylene
Injection molded parts.Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 66.0 °C
151 °F
50°C/hr; 50N
Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy ..
Vicat Softening Point 66.0 °C
151 °F
ASTM D1525
Arkema Group OREVAC® 9307 Y EVA Terpolymer
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre..
Vicat Softening Point 66.0 - 113 °C
151 - 235 °F
Average value: 97.4 °C Grade Count:34
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..