Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 88.0 - 99.0 °C | 190 - 210 °F | ISO 306A |
Ineos Nova 602 Crystal Polystyrene GP Grade
(discontinued **) Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise spe.. |
|||
Vicat Softening Point | 35.0 - 99.0 °C | 95.0 - 210 °F | Average value: 76.9 °C Grade Count:41 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Vicat Softening Point | 97.0 - 99.0 °C | 207 - 210 °F | Average value: 97.3 °C Grade Count:6 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |