Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 109 °C | 228 °F | ASTM D3418 |
ExxonMobil LL 3002.32 Cast Film Resin
(discontinued **) LL 3002.32 is a hexene copolymer LLDPE cast film resin. Films produced from this resin have excellent tensile properties, as well as stiffness and toughness. Combined with good drawdown properties, .. |
|||
Crystallization Temperature | 109 °C | 228 °F | ExxonMobil Method |
ExxonMobil NTX™ NTX 101 Super Strength Film Resin NTX 101 is a super strength hexene copolymer LLDPE film resin. Films made from this resin have outstanding toughness properties, especially impact and tear strength, compared to other hexene copoly.. |
|||
Crystallization Temperature | 109 °C | 228 °F | Dow Method (DSC) |
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D.. |
|||
Crystallization Temperature | 109 °C | 228 °F | Dow Method (DSC) |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Crystallization Temperature | 109 - 113 °C | 229 - 235 °F | Average value: 111 °C Grade Count:8 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |