Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 49.0 °C | 120 °F | DSC, 10°C/min (peak); DuPont Test |
Dow Engage® ENR 7270.00 Ethylene-Butene Copolymer Description: ENR 7270.00 is a general purpose ethylene-butene copolymer designed to provide good cost/performance balance in polymer modification applications.Information provided by manufacturer.Th.. |