Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 130 °C | 266 °F | Melting; DSC |
LG Chemical LUTENE-H ME6000 HDPE Description: LUTENE-H ME6000 is mainly intended for injection molding of crates. It has excellent mechanical properties and high impact strength.Applications: Transport and stacking crates, bottle c.. |