Thermal Properties Metric English Comments
Crystallization Temperature 85.0 - 96.0 °C
185 - 205 °F
Average value: 90.9 °C Grade Count:16
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..