Polymer Property : Crystallization Temperature = 232.2 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 111.2 °C
232.2 °F
ASTM D3418
ExxonMobil LL 8360 Rotational Molding Resin  (discontinued **)
LL 8360 is a linear low density hexene copolymer designed to provide good processability along with outstanding dimensional control and low warpage. This resin is ideally suited for applications tha..