Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 112.1 °C | 233.8 °F | ASTM D3418 |
ExxonMobil LL 8555.67 Rotational Molding Resin
(discontinued **) LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir.. |