Polymer Property : Crystallization Temperature = 237 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 112 - 114 °C
234 - 237 °F
Average value: 113 °C Grade Count:4
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu..