Thermal Properties Metric English Comments
Crystallization Temperature 115.8 °C
240.4 °F
ASTM D3418
LyondellBasell Alathon® M5372 High Density Polyethylene
ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. ..