Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 136 °C | 277 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Sol.. |
|||
Crystallization Temperature | 136 °C | 277 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF) Solef® 42308 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Solvay S.. |
|||
Crystallization Temperature | 136 °C | 277 °F | Peak, DSC; ASTM D3418 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Information provided by Solvay Specialty Polymers. |