Polymer Property : Crystallization Temperature = 295 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 295 °C
563 °F
Peak; ASTM D3418
Solvay Specialty Polymers Hyflon® PFA 120 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Crystallization Temperature 295 °C
563 °F
Peak; ASTM D3418
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Crystallization Temperature 295 °C
563 °F
Peak, DSC
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)  (discontinued **)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis..
Crystallization Temperature 295 °C
563 °F
Peak, DSC
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis..