Polymer Property : Crystallization Temperature = 50.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 35.0 - 50.0 °C
95.0 - 122 °F
Addcomp PRIEX® 25050 Maleic Anhydride Grafted PP random copolymer
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..
Crystallization Temperature 35.0 - 50.0 °C
95.0 - 122 °F
Addcomp PRIEX® 25095 Maleic Anhydride Grafted PP random copolymer
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..