Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 285 - 295 °C | 545 - 563 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |