Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -23.7 °C | -10.7 °F | Retraction Temperature, TR10; ASTM D1329 |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Minimum Service Temperature, Air | -23.7 °C | -10.7 °F | Retraction Temperature, TR10; ASTM D1329 |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |