Thermal Properties Metric English Comments
Minimum Service Temperature, Air -13.5 °C
7.70 °F
Gehman torsion test, T10
Daikin DAI-EL G-558 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content
Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low gasoline permeability and good..