Thermal Properties Metric English Comments
Minimum Service Temperature, Air -115 - -40.0 °C
-175 - -40.0 °F
Average value: -68.5 °C Grade Count:32
Overview of materials for Silicone, RTV, Encapsulation Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value..
Minimum Service Temperature, Air -115 °C
-175 °F
Continuous useful temperature.
Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Minimum Service Temperature, Air -115 °C
-175 °F
Continuous useful temperature.
Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Minimum Service Temperature, Air -115 °C
-175 °F
Continuous useful temperature.
Momentive Performance Materials RTV560 Red Extreme High Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Minimum Service Temperature, Air -115 °C
-175 °F
Continuous useful temperature.
Momentive Performance Materials RTV566 Red Extreme High Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Minimum Service Temperature, Air -115 °C
-175 °F
Continuous useful temperature.
Momentive Performance Materials RTV567 Translucent Extreme Low Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Minimum Service Temperature, Air -115 °C
-175 °F
Continuous useful temperature.
Momentive Performance Materials RTV6156 Clear Potting/Encapsulating Gel
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..
Minimum Service Temperature, Air -115 °C
-175 °F
Continuous useful temperature.
Momentive Performance Materials RTV656 Clear Extreme Low Temperature Potting/Encapsulating Compound
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..
Minimum Service Temperature, Air -115 °C
-175 °F
ACC QSil 940 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting
QSil 940 is a special purpose, two-component condensation cure siloxane elastomer that exhibits excellent release properties unless a primer is used which results in excellent adhesion. The material..