Thermal Properties Metric English Comments
Minimum Service Temperature, Air -19.0 °C
-2.20 °F
TR test, TR10
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content
Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries.